FSK - Hardcore Evo Heatmoulding Tutorial

FSK - Hardcore Evo Heatmoulding Tutorial If you want to improve the fit of your Powerslide Hardcore Evo skate, you have the option to heatmold them. This simple tutorial will show you how to heatmould correctly. First, take the wheels off your skates. The frame should stay mounted on the boot. Pre-heat your oven to 100 - 110 °C / 210 - 230 °F. Place your boots in the oven for about 20 minutes. Make sure the boot are not placed to close to the heat source of your oven. After 20 minutes, take the skate out